Back to Ice769
Forward to Ice771
Categories
Prev in series (769) Next in Marsden series(771)

Ice770: std ice; Seidemann/Prior stress drop study

T = 240 K, P = 50 MPa, s = 13.4 MPa to e = 0.15 step (1)
T = 240 K, P = 50 MPa, s = 3 MPa to e = 0.24 step (2)
after deformation

 

 

run_summary

micrographs

(not yet)

run_log
    other resources: live updates (archived)

 

step (1) (cf. 748)
step (1)
step (2)