Equipment
Lab and Coral NameTRL / Balzer-Elionix
ModelBalzer
SpecialistDennis Ward     (Paul Tierney)
Physical Location4F External-Photo
Classification
Process CategoryDeposition
SubcategorySputter
Material KeywordsNon-CMOS Metals
Sample SizePieces
AlternativeTRL / AJA-TRL, TRL / eBeamFP, TRL / eBeamAu
Keywordsmanual load, top side of sample, conformal dep, vacuum, plasma, manual operation
Description
The Balzer-Elionix is primarily used to sputter thin layer of Au. One application is to prevent prevent charging effects on insulating substrates in SEM, ebeam lithography. This tool is simple and fast for this purpose compared to alternatives.

Best forApplications require thin layer of Au, such as preventing charging effects in SEM, ebeam lithography on insulating substrates.
LimitationsAu only, thin layers.
Characteristics/FOM
Caution withPotential adhesion problem of Au, as no adhesion layers can be deposited with this tool.
Machine Charges8/hour
Documents
Process Matrix Details

Permitted
Been in the ALDSamples that have been in any of the ALD systems
,
Pyrex SubstratesPyrex substrates can be a concern due to high sodium content, which contaminates CMOS frontend tools
,
III-V SubstratesAny III-V substrates, e.g. GaAs, GaN, InP, and so on. Note though that many common III-V substrates will also carry the Au flag, but there are some GREEN III-V substrates.
,
Germanium on surfaceSamples with germanium on the surface (typically grown films)
,
Germanium buriedSamples with germanium buried below a different film
,
PiecesWafer pieces may not be handled by the equipment, and are harder to thoroughly clean - preventing them from running in certain tools.
,
Gold or RED color codeRED color code substrates. These are gold-contaminated or have been processed in gold contaminated tools. Gold and other metals can contaminate silicon devices (GREEN color code) and have to be separated.
(Adds),
Any exposure to CMOS metalIf the sample had ever seen a CMOS metal (or a tool that accepts CMOS metal), then some frontend tools could be contaminated by this.
,
CMOS metal on surfaceCMOS compatible metals exposed on the surface. These are Al,Ni,Pt,Ti,TiN. Other metals such as Au are *NOT* part of this.
,
CMOS metal buriedCMOS compatible metals covered entirely by a different material. These are Al,Ni,Pt,Ti,TiN. Other metals such as Au are *NOT* part of this.
,
Been in the STS DRIEThe DRIE etch leaves behind polymer residues on the sidewall ripples, which can be a contamination concern for some tools.
,
Been in the SEMA sample viewed in the SEM must have used the appropriate chuck to avoid cross-contamination
,
Been in the Concept1The Concep1 deposits dielectrics on GREEN wafers, however it also accepts metal and there can be cross-contamination for diffusion area
,
Has PhotoresistSamples with photoresist cannot be exposed to high temperatures, which is typical in deposition tools. Outgassing can be a concern.
,
Has PolyimidePolyimide is a very chemically resistant polymer, and can tolerate higher temperatures but cannot be exposed to typical PECVD deposition temperatures or diffusion furnaces. Outgassing can be a concern.
,
Has Cured SU8Not fully cured SU8 residues can heavily contaminated plasma chambers or destroy other user's samples, but fully cured SU8 is permitted in certain tools.
,
Coming from KOHAfter a KOH etch, the samples must receive a special clean because the K ions are highly contaminating to CMOS frontend tools
,
Coming from CMPAfter a CMP, the samples must receive a special clean, because the slurry residues otherwise introduce contamination and particles.


Not Allowed
Ever been in EMLSamples from EML are never permitted to return to ICL or TRL


For more details or help, please consult PTC matrix, email ptc@mtl.mit.edu, or ask the research specialist (Dennis Ward )